无机材料学报

• 研究论文 • 上一篇    下一篇

锐钛矿型TiO2纳米粉的低温热容研究

吴新明1,2; 邸友莹1,2; 谭志诚2; 屈松生1   

  1. 1. 武汉大学化学与环境科学学院, 武汉 430072; 2. 中国科学院大连化学物理研究所, 大连 116023
  • 收稿日期:2000-02-28 修回日期:2000-04-24 出版日期:2001-01-20 网络出版日期:2001-01-20

Low Temperature Heat Capacity of the Anatase Nano-Powder TiO2

WU Xin-Ming1,2; DI You-Ying1,2; TAN Zhi-Cheng2; QU Song-Sheng 1   

  1. 1.College of Chemistry and Environmental Science; Wuhan University; Wuhan 430072; China; Thermochemistry Laboratory; Dalian Institute of Chemical Physics; Chinese Academy of Sciences; Dalian 116023; China
  • Received:2000-02-28 Revised:2000-04-24 Published:2001-01-20 Online:2001-01-20

摘要: 采用溶胶-凝胶法制备了16、26nm锐钛矿型TiO纳米晶超微粉末,测定了其纳米尺寸和晶态.在78~370K温区测定了热容,拟合出热容随温度变化的多项式方程,并与锐态矿型粗晶TiO热容文献值进行比较,从能量不同的角度分析了各曲线不同的原因.

关键词: 锐钛矿型TiO2, 纳米晶超微粉, 溶胶-凝胶法, 低温热容

Abstract: The nanocrystalline TiO2 ultrafine powders in anatase phase were prepared in 16nm, 26nm
by means of a sol-gel method. The particle sizes and the crystallographic phase were determined. Heat capacities in the temperature range of
78~370K were also measured, and the polynomial equations expressing the change of heat capacity with temperature were fitted. The obtained
values of the heat capacity were compared with those of the coarse crystal from the literature. The relationship between heat capacities and the
particle sizes of nanocrystalline TiO2 were demonstrated in the view of energetics.

Key words: anatase phase TiO2, nanocrystalline ultrafine powder, sol-gel method, low-temperature heat capacity

中图分类号: