TiB2/TiC Nano-Composite Powder Fabricated via High Energy Milling

LI Jian-Lin1; CAO Guang-Yi2; ZHOU Yong1; HU Ke-Ao 1   

  1. 1.State key lab of metal matrix composites; Shanghai Jiaotong University; Shanghai 200030; China; 2. Shanghai Jiaotong University, Shanghai, China
  • Received:2000-06-26 Revised:2000-07-11 Published:2001-07-20 Online:2001-07-20

Abstract: The process and the mechanism of TiB2/TiC nano-composite powder fabricated via high energy milling were studied, and as-prepared powders were characterized by TIM and XRD techniques. The results show that Ti can react with B4C during milling process, and TiC is firstly produced, TiB2/TiC particles formed after 5 hours milling. TiB2 and TiC phases co-exist in following long time milling. After 30 hours milling, nanosized TiC particles with a diameter of 8 urn are located in TiB2 particles with a size of 100-200nm.

Key words: high energy milling, boron carbide, titanium carbide, titanium boron