无机材料学报 ›› 2013, Vol. 28 ›› Issue (10): 1108-1114.DOI: 10.3724/SP.J.1077.2013.12755 CSTR: 32189.14.SP.J.1077.2013.12755

• 研究论文 • 上一篇    下一篇

YSZ/Ni-YSZ双层中空纤维电解质层厚度控制及其影响

宫 勋1, 孟秀霞1,2, 杨乃涛1, 谭小耀1,3, 尹屹梅2, 马紫峰2   

  1. (1. 山东理工大学 化工学院, 淄博 255049; 2. 上海交通大学 化学工程系, 上海200240; 3. 天津工业大学 化学工程系, 天津300160)
  • 收稿日期:2012-12-14 修回日期:2013-01-22 出版日期:2013-10-20 网络出版日期:2013-09-18
  • 作者简介:宫 勋(1987-), 男, 硕士研究生. E-mail:ash1025@126.com
  • 基金资助:

    国家自然科学基金(21176187, 21076118, 21173147); 山东省优秀中青年科学家科研奖励基金(2010BSB01011)

Electrolyte Thickness Control and Its Effect on YSZ/Ni-YSZ Dual-layer Hollow Fibres

GONG Xun1, MENG Xiu-Xia1, 2, YANG Nai-Tao1, TAN Xiao-Yao1,3, YIN Yi-Mei2, MA Zi-Feng2   

  1. (1 School of Chemical Engineering, Shandong University of Technology, Zibo 255049, China; 2 Institute of Electrochemical & Energy Technology, Shanghai Jiao Tong University, Shanghai 200240, China; 3 Department of Chemical Engineering, Tianjin Polytechnic University, Tianjin 300160, China)
  • Received:2012-12-14 Revised:2013-01-22 Published:2013-10-20 Online:2013-09-18
  • About author:GONG Xun. E-mail:ash1025@126.com
  • Supported by:

    National Natural Science Foundation of China (21176187, 21076118, 21173147); Promotive Research Fund for Excellent Young and Middle-aged Scientists of Shandong Province (2010BSB01011)

摘要: 本研究利用相转化共纺丝法一步制备出微管式固体氧化物燃料电池(MT-SOFC)用电解质/阳极(YSZ/NiO-YSZ)双层中空纤维膜, 将制得的YSZ/NiO-YSZ双层中空纤维膜前驱体经1450℃烧结后, 以纯H2在700℃下还原4 h得到YSZ/Ni-YSZ双层中空纤维膜。电解质YSZ膜层厚度通过改变YSZ铸膜液挤出速率来调节。将La0.8Sr0.2MnO3-δ(LSM)阴极乳浆浸渍涂覆在烧结后的YSZ/NiO-YSZ双层中空纤维膜外, 经1200℃烧结后形成微管式固体氧化物燃料电池。结果表明, 当阳极铸膜液以10?mL/min速率挤出, 而电解质铸膜液挤出速率为0.5、1、1.5、2 mL/min时, 构造的YSZ/Ni-YSZ双层中空纤维膜电解质层厚度分别为6、13、18、28 μm, 其机械强度、气密性均随着电解质层厚度增加而增大, 但电导率与孔隙率受电解质层厚度的影响较小。YSZ膜厚度为28 μm的MT-SOFC, 800℃时以20 mL/min氢气作为燃料, 30 mL/min空气作为氧化剂, 最大开路电压为1.01 V, 最大输出功率只有75 mW/cm2。但同样测试条件下, YSZ膜厚度为6 μm的MT-SOFC, 开路电压为0.92 V, 最大输出功率升至329 mW/cm2

关键词: 双层中空纤维, YSZ电解质膜, 相转化法, 微管式固体氧化物燃料电池, 共纺丝-共烧结

Abstract: Electrolyte/anode (YSZ/NiO-YSZ) dual-layer hollow fibres were developed by a co-spinning process based on phase inversion technique for fabrication of micro tubular solid oxide fuel cells (MT-SOFCs). After being calcined at 1450℃ in ambient air and reduced at 700℃ in H2 for 4 h, the precursors were transformed into dual layer YSZ/Ni-YSZ hollow fibers. Full MT-SOFCs were fabricated by dip-coating with La0.8Sr0.2MnO3-δ (LSM) ink on the outer surface of YSZ/NiO-YSZ dual layer hollow fibers and sintering at 1200℃. The results show that the YSZ membranes of the dual-layer hollow fibers possess thicknesses of 6, 13, 18 and 28 μm when the spinning rates of electrolyte dopes are 0.5, 1, 1.5 and 2 mL/min and the anode dope keeps on a constant rate of 10 mL/min. The bending strength and the gas-tightness of the dual-layer hollow fibers increase with the increase of electrolyte thickness. However, the electrical conductivity and porosity of the dual-layer hollow fibers are less influenced by YSZ thickness. The maximum power density of single MT-SOFC with an electrolyte layer of 28 μm is 75 mW/cm2, while the output of an MT-SOFC with a 6 μm-thick YSZ membrane is up to 329 mW/cm2, both operated at 800?℃ using 20 mL/min H2 as fuel and 30 mL/min air as oxidant.