Tantalum carbide materials were prepared by liquid precursor conversion, and the phase compositions and the microscopic structures of samples were characterized by XRD and SEM, respectively. Ta2O5 crystals are formed inside samples by 900℃ treatment, and after 1600~2000℃ high temperature treatment, the samples can almost be converted into tantalum carbide materials whose particles disperse homogeneously throughout the carbon matrix. As temperatures elevate, the graphitization degree of matrix increases and the grain size of tantalum carbide obviously enlarges, all of these are in favor of improving the anti-ablation properties of materials.
XIANG Hua
,
XU Yong-Dong
,
ZHANG Li-Tong
,
CHENG Lai-Fei
. Preparation of TaC Anti-ablation Materials by Liquid Precursor[J]. Journal of Inorganic Materials, 2006
, 21(4)
: 893
-898
.
DOI: 10.3724/SP.J.1077.2006.00893
1 林德春, 张德雄, 陈继荣. 宇航材料工艺, 1994, 24(4): 1-5.
2 苏君明. 新型碳材料, 1996, 11(3): 18-23.
3 苏君明. 第18届炭-石墨材料学术会议论文集, 2000. 198-207.
4 宋桂明, 周玉, 王玉金, 等. 固体火箭技术, 1998, 21(2): 51-61.
5 倪礼忠, 陈麒. 复合材料科学与工程, 第一版. 北京: 科学出版社, 2002. 171-175.
6 Preiss H, Schultze D, Klobes P. Journal of the European Ceramic Society, 1997, 17(12): 1423-1435.
7 Kevin Thorne, Eric Liimatta, John D. Journal of Material Research, 1991, 6(10): 2199-2207.
8 陈冠荣, 等. 化工百科全书(第十五卷), 第一版. 北京: 化学工业出版社, 1997. 635-642.
9 何万年. 新疆有色金属, 2000, 4: 28-32.
10 何捍卫, 周科朝, 熊翔. 稀有金属材料与工程, 2004, 33(5): 490-493.
11 崔红, 苏君明, 李瑞珍, 等. 西北工业大学学报, 2000, 18(4): 669-673.
12 Chen Yong-Jun, Li Jian-Bao, Wei Qiang-Min, et al. Journal of Crystal Growth, 2001, 224(3-4): 244-250.