Thermal Stability Investigation of a Newly Developed Sealing Glass as IT-SOFC Sealant

  • PENG Lian ,
  • ZHU Qing-Shan ,
  • XIE Zhao-Hui ,
  • HUANG Wen-Lai
Expand
  • 1. Multiphase Reaction Lab, Institute of Process Engineering, Chinese Academy of Sciences, Beijing 100080, China;
    2. Graduate School of the Chinese Academy of Sciences, Beijing 100049, China

Received date: 1900-01-01

  Revised date: 1900-01-01

  Online published: 2006-07-20

Abstract

A sealing glass, based on the SiO2-B2O3-BaO-La2O3-ZrO2-Y2O3 system, was developed for intermediate temperature solid oxide fuel cells (ITSOFCs). The coefficient of thermal expansion (CTE) of the glass is 9.8×10-6/K (RT~631℃), very close to that of 8YSZ electrolyte. The glass shows a very good thermal stability, even after heat-treatment at 700℃ for 300h, little change in CTE detected. The investigations also reveal that the glass is chemically compatible with 8YSZ electrolyte and no obvious interfacial reaction can be observed after the glass contacting with 8YSZ at 700℃ for 300h.

Cite this article

PENG Lian , ZHU Qing-Shan , XIE Zhao-Hui , HUANG Wen-Lai . Thermal Stability Investigation of a Newly Developed Sealing Glass as IT-SOFC Sealant[J]. Journal of Inorganic Materials, 2006 , 21(4) : 867 -872 . DOI: 10.3724/SP.J.1077.2006.00867

References

1 Yang Z G, Stevenson J W, Meinhardt K D. Solid State Ionics, 2003, 160: 213-225.
2 Schwickert T, Sievering R, Geasee P, et al. Materialwiss Werkst, 2002, 33: 363-366.
3 Loehman R E, Dumm H P, Hofer H. Ceramic Engineering and Science Proceedings, 2002, 23 (3): 699-710.
4 Weil K S, Coyle C A, Hardy J S, et al. Fuel Cells Bulletin, 2004, 5: 11-16.
5 Bram M, Reckers S, Drinovac P, et al. Electrochemical Society Proceedings, 2003, 7: 888-897.
6 Ley K L, Krumpelt M, Kumar R, et al. Journal of Materials Research, 1996, 11 (6): 1489-1493.
7 Eichler K, Solow G, Otschik P, et al. Journal of the European Ceramic Society, 1999, 19: 1101-1104.
8 Sohn S B, Choi S Y, Kim G H, et al. Journal of American Ceramic Society, 2004, 87 (2): 254-260.
9 郑锐, 等(ZHENG Rui, et al). 无机材料学报(Journal of Inorganic Materials),
2004, 19(1): 37-42.
10 Sohn S B, Choi S Y, Kim G H, et al. Journal of Non-Crystalline solids, 2002, 297: 103-112.
11 Zheng R, Wang S R, Nie H W, et al. Journal of Power Sources, 2004, 128: 165-172.
12 Tuller H L, Schoonman J, Riess l. Oxygen Ion and Mixed Conductors and their Technological Applications. Netherlands: Kluwer Academic Publishers, 2000. 389-397.
13 Taniguchi S, Kadowaki M, Yasuo T, et al. Journal of Power Sources, 2000, 90: 163-169.
14 Lahl N, Singheiser L, Hilpert K, et al. Electrochemical Society Proceedings, 1999, 99 (19): 1057-1066.
15 Lahl N, Singh K, Singheisier L, et al. Journal of Materials Science, 2000, 35: 3089-3096.
16 Larsen P H, James P F. Journal of Materials Science, 1998, 34: 2499-2507.
17 朱庆山, 彭练, 黄文来, 谢朝晖. 一种固体氧化物燃料电池密封策略及密封玻璃. 中国发明专利, 02124834.6, 2005.
Outlines

/