Kinetic Research of Oxidation Induced Crack Healing of Engineering Ceramics (Ⅲ) Model Testing and Revising: The Kinetic Research of Al2O3-SiC W Composite

  • Lü Jun ,
  • ZHENG Zhi-Xian ,
  • WU Yu-Cheng ,
  • JIN Zhi-Hao
Expand
  • 1. Materials Science and Engineering Institute, Hefei University of Technology,
    Hefei 230009, China;
    2. State Key Laboratory for Mechanical Behvior of Materials, Xi'an Jiaotong University, Xi'an 710049, China

Received date: 2004-12-02

  Revised date: 2005-02-06

  Online published: 2006-05-20

Abstract

Oxidation reaction happened when Al2O3-SiC W composite heated at high temperature. The reaction producer moved to the crack area which induced crack healing. The kinetic analysis of crack healing of Al2O3-SiC W composite shows that: the velocity of crack healing can be showed as: - Cv/t=(2πC2v0·ΔP+F)/(2πB0Cv)·1/2·(k/t)1/2, and the strength recovery can be expressed by the following formula: σff0=[1-(2πC2v0·ΔP+F)/(πB0C2v0)·k1/2·t1/2]-1/4. Compared with Al2O3-TiC P composite, the filling coefficient F was added. The physical meaning of F coefficient is the area equivalent except the crack area. For Al2O3-SiC W composite, F is related to the whisker bridge, whisker emerge, and the area on which reaction producer can follow and fill in the crack. When heated at 1200℃, F is about 9.94\times10-8 m2.

Cite this article

Lü Jun , ZHENG Zhi-Xian , WU Yu-Cheng , JIN Zhi-Hao . Kinetic Research of Oxidation Induced Crack Healing of Engineering Ceramics (Ⅲ) Model Testing and Revising: The Kinetic Research of Al2O3-SiC W Composite[J]. Journal of Inorganic Materials, 2006 , 21(3) : 696 -700 . DOI: 10.3724/SP.J.1077.2006.00696

References

1 Jun Lv, Zheng Zh X, Ding H F, et al. Jin. Fatigue & Fracture of Engineering Materials & Structures, 2004, 27(2): 89-97.
2 Chiu Chin-Chen. J. Mater. Sci., 1994, 29: 2078-2082.
3 Krishan L Luthra, Hee Dong Park. J. Am. Ceram. Soc., 1990, 73(4): 1014-1023 .
4 吕珺, 郑治祥, 金志浩. 复合材料学报, 2001, (4): 76-81.
5 Zheng Z, Tressler R E, Spear K E. J. Electrochem. Soc., 1990, 137(3): 854-858.
6 Zheng Z, Tressler R E, SpearK E. J. Electrochem. Soc., 1990, 137(9): 2812-2816.
7 Monika Backhaus-Ricoulf. J. Am. Ceram. Soc., 1991, 74(8): 1793-1802.
Outlines

/