High temperature electrical conductivity of perovskite-type mixed with ionic-electronic conductor La0.6Sr0.4Co0.2Fe0.8O3–δ (LSCF) and La0.6Sr0.4Co0.2Fe0.8O3–δ- Ce0.9Gd0.1O1.95(LSCF-GDC) composite material were studied by the DC four-terminal technique. The activation energies of pure LSCF and LSCF-GDC composite for small polaron conduction were Ea1=9.72kJ/mol and Ea2=10.64kJ/mol, respectively. Through electrical conductivity relaxation method, i.e. a continuously resistance measurement during the sudden change oxygen under partial pressure and the surface exchange property of the two samples were also investigated. In the temperature range from 600℃ to 800℃ and the oxygen partial pressure range from 21kPa to 34kPa, the oxygen surface exchange coefficients (kchem) were determined as 2.87×10-6-6.91×10-6cm/s. It is the catalysis effects of GDC on oxygen surface exchange process and the microstructure effect of introducing GDC that promoted the oxygen transport process of composite materials jointly. Based on the relationship of kchem and temperature, the activation energies for surface exchange process was also estimated.
WANG Yan-Dong 1
,
2
,
LV Zhe 2
,
WEI Bo 2
. High Temperature Electrical Relaxation Study of La0.6Sr0.4Co0.2Fe0.8O3–δ-Ce0.9Gd0.1O1.95 Composite[J]. Journal of Inorganic Materials, 2010
, 25(6)
: 635
-640
.
DOI: 10.3724/SP.J.1077.2010.00635
[1]张国光, 刘 卫, 谢津桥, 等(ZHANG Guo-Guang, et al). SrFe1.5-xCoxOy混合导体的制备及氧化扩散研究.硅酸盐学报(Chinese Journal of Ceramic Society), 2000, 28(1): 20-24.
[2]刘 卫, 章占平, 夏长荣, 等(LIU Wei, et al). 多孔 La0.6Sr0.4Co0.2Fe0.8O3-δ的制备及表征.无机材料学报(Journal of Inorganic Materials), 2000, 15(5): 849-854.
[3]李 艳, 吕 喆, 王洪涛, 等(LI Yan, et al).固体氧化物燃料电池梯度复合阴极材料的制备及性能研究.无机材料学报(Journal of Inorganic Materials), 2007, 22(5): 885-888.
[4]Wang S, van der Heide P A W, Chavez C, et al. An electrical conductivity relaxation study of La0.6Sr0.4Fe0.8Co0.2O3-δ. Solid State Ionics, 2003, 156(1/2): 201-208.
[5]Esquirol A, Kilner J, Brandon N. Oxygen transport in La0.6Sr0.4Co0.2Fe0.8O3-δ/Ce0.8Ge0.2O2-x composite cathode for IT-SOFCs. Solid State Ionics, 2004, 175(1/2): 63-67.
[6]Dusastre V, Kilner J A. Optimisation of composite cathodes for intermediate temperature SOFC applications. Solid State Ionics, 1999, 126(1/2): 163-174.
[7]Bucher E, Jantscher W, Benisek A, et al. Transport properties of La0.6Sr0.4CoO3-δ. Solid State Ionics, 2001, 141-142: 375-380.
[8]Ganeshananthan R, Virkar A V. Measurement of surface exchange coefficient on porous La0.6Sr0.4CoO3-δ samples by conductivity relaxation. J. Electrochem. Soc., 2005, 152(8): A1620-A1628.
[9]Kostogloudis G C, Ftikos C. Properties of A-site-deficient La0.6Sr0.4Fe0.8Co0.2O3-δ-based perovskite oxides. Solid State Ionics, 1999, 126(1/2): 143-151.
[10]黄端平, 徐 庆, 陈 文, 等(HUANG Duan-Ping, et al). La0.6Sr0.4Co1-yFeyO3的混合导电性研究. 无机材料学报(Journal of Inorganic Materials), 2005, 20(1): 133-138.
[11]Tai L W, Nasrallah M M, Anderson H U, et al. Structure and electrical properties of La0.6Sr0.4Co1-yFeyO3. Solid State Ionics, 1995,76(3/4): 259-271.