Research Paper

Preparation and Application of Perovskite Hollow Fiber Oxygen Permeable Membrane

  • CHEN Xin-Zhi ,
  • YU Ling-Hui ,
  • LIU Qiao-Sheng ,
  • WANG Hai-Hui ,
  • LI Zhong
Expand
  • School of Chemistry & Chemical Engineering, South China University of Technology, Guangzhou 510640, China

Received date: 2008-01-07

  Revised date: 2008-03-14

  Online published: 2008-11-20

Abstract

The dense perovskite hollow fiber made of BaCo0.4Fe0.4Zr0.2O3-δ (BCFZ) was prepared by phase inversion spinning followed by sintering. The crystal structure and the microstructures of the hollow fiber membrane were characterized by X-ray diffraction (XRD) and scanning electron microscope (SEM). The sintered hollow fiber membrane was also used to construct a reactor for the partial oxidation of methane (POM) to syngas. It is found that the BCFZ itself exhibits low activity for conversion of methane which is lower than 3% without catalysts. After Ni-based catalyst is introduced, the conversion of methane, the CO selectivity and the oxygen permeation flux reach 93%, 80% and 11mL/min·cm2, respectively. It takes only 90min to get the steady state at initial stage in the hollow fiber membrane reactor, which is much shorter than that in the disk-type membrane reactor. The hollow fiber membrane reactor is steadily operated for 40h for the POM reaction.

Cite this article

CHEN Xin-Zhi , YU Ling-Hui , LIU Qiao-Sheng , WANG Hai-Hui , LI Zhong . Preparation and Application of Perovskite Hollow Fiber Oxygen Permeable Membrane[J]. Journal of Inorganic Materials, 2008 , 23(6) : 1216 -1220 . DOI: 10.3724/SP.J.1077.2008.01216

References

[1] Teraoka Y, Zhang H M, Furuka S, et al. Chem. Lett., 1985, 11 (14): 1743-1746.
[2] Chen C S, Liu W, Xie S, et al. Adv. Mater., 2000, 12 (15): 1132-1134.
[3] Balachandran U, Dusek J T, Maiya P S, et al. Catal. Today, 1997, 36 (3): 265-272.
[4] Yi J X, Zuo Y B, Liu W, et al. J. Membr. Sci., 2006, 280 (1-2): 849-855.
[5] Chen C S, Feng S J, Ran S, et al. Angew. Chem. Int. Ed., 2003, 42 (42): 5196-5198.
[6] Wu Z T, Jin W Q, Xu N P. J. Membr. Sci., 2006, 279 (1-2): 320-327.
[7] Li S G, Jin W Q, Huang P, et al. AIChE J., 1999, 45 (2): 276-284.
[8] Pei S, Kleefisch M S, Kobylinski T P, et al. Catal. Lett., 1994, 30 (1-4): 201-208.
[9] Gu X H, Jin W Q, Chen C L, et al. AIChE J., 2002, 48 (9): 2051-2060.
[10] Shao Z P, Yang W S, Cong Y, et al. J. Membr. Sci., 2000, 172 (1-2): 177-188.
[11] Tong J H, Yang W S, Zhu B C, et al. J. Membr. Sci., 2002, 203 (1-2): 175-189.
[12] Dong H, Shao Z P, Xiong G X, et al. Catal. Today, 2001, 67 (1-3): 3-13.
[13] Shao Z P, Dong H, Xiong G X, et al. J. Membr. Sci., 2001, 183 (2): 181-192.
[14] Hu J, Hao H S, Chen C P, et al. J. Membr. Sci., 2006, 280 (1-2): 809-814.
[15] 宋红章, 杨德林, 胡 婕, 等(SONG Hong-Zhang, et al). 无机材料学报(Journal of Inorganic Materials), 2006, 21 (1): 199-203.
[16] 谭小耀, 孟 波, 杨乃涛(TAN Xiao-Yao, et al). 无机材料学报(Journal of Inorganic Materials), 2006, 21 (1): 245-249.
[17] Zhang C, Xu Z, Chang X F, et al. J. Membr. Sci., 2007, 299 (1-2): 261-267.
[18] Wang B, Zhu D C, Zhan M C, et al. AIChE J., 2007, 53 (9): 2481-2484.
[19] Liu S, Gavalas G R. J. Membr. Sci., 2005, 246 (1): 103-108.
[20] Liu S, Gavalas G R. Ind. Eng. Chem. Res., 2005, 44 (20): 7633-7637.
[21] Tan X Y, Liu Y, Li K. AIChE J., 2005, 51 (7): 1991-2000.
[22] Tan X Y, Liu Y, Li K. Ind. Eng. Chem. Res., 2005, 44 (1): 61-66.
[23] Tan X Y, Li K. Ind. Eng. Chem. Res., 2006, 45 (1): 142-149.
[24] Tablet C, Grubert G, Wang H H, et al. Catal. Today, 2005, 104 (2-4): 126-130.
[25] Wang H H, Werth S, Schiestel T, et al. Angew. Chem. Int. Ed., 2005, 44 (42): 6906-6909.
[26] Schiestel T, Kilgus M, Peter S, et al. J. Membr. Sci., 2005, 258 (1-2): 1-4.
[27] Wang H H, Tablet C, Schiestel T, et al. Catal. Commun., 2006, 7 (11): 907-912.
[28] Kleinert A, Feldhoff A, Schiestel T, et al. Catal. Today, 2006, 118 (1-2): 44-51.
Outlines

/