Research Paper

Mechanical Properties of C/SiC/Si-Mo-Cr Multilayer Coated Carbon/carbon Composites

  • ZHANG Yu-Lei ,
  • LI He-Jun ,
  • YAO Xi-Yuan ,
  • FU Qian-Gang ,
  • LI Ke-Zhi
Expand
  • C/C Composites Technology Research Center, Northwestern Polytechnical University, Xi’an 710072, China

Received date: 2007-08-22

  Revised date: 2007-10-15

  Online published: 2008-07-20

Abstract

A novel C/SiC/Si-Mo-Cr multilayer oxidation protective coating for carbon/carbon composites was prepared by pack cementation and slurry method. The microstructures of the as-prepared multilayer coating were characterized by XRD and SEM analyses. The effects of the coating processing and thermal shock on the mechanical properties of carbon/carbon composites were investigated by three point bending tests. The results show that the asobtained multiphase coating is dense, and the flexural strength of carbon/carbon composites after coating increases and the fracture behavior changes from the pseudoplastic fracture to brittle fracture mode. After enduring the thermal cycling between 1500℃ and room temperature for 20 cycles, the flexural strength of the coated specimens decreases accordingly, and the plastic increases.

Cite this article

ZHANG Yu-Lei , LI He-Jun , YAO Xi-Yuan , FU Qian-Gang , LI Ke-Zhi . Mechanical Properties of C/SiC/Si-Mo-Cr Multilayer Coated Carbon/carbon Composites[J]. Journal of Inorganic Materials, 2008 , 23(4) : 725 -728 . DOI: 10.3724/SP.J.1077.2008.00725

References

[1] Buckley J D. Ceram. Bull., 1988, 67 (2): 364-368.
[2] 易法军, 孟松鹤, 韩杰才, 等(YI Fa-Jun, et al). 无机材料学报(Journal of Inorganic Materials), 2001, 16 (6): 1229-1234.
[3] 李贺军. 新型炭材料, 2001, 16 (2): 79-80.
[4] Westwood M E, Webster J D, Day R J, et al. J. Mater. Sci., 1996, 31 (6): 1389-1397.
[5] Luthra K L. Carbon, 1988, 26 (2): 217-224.
[6] 牛晓滨, 廖 源, 常 超, 等(NIU Xiao-Bin, et al). 无机材料学报(Journal of Inorganic Materials), 2004, 19 (2): 397-402.
[7] Smeacetto F, Ferraris M, Salvo M. Carbon, 2003, 41 (11): 2105-2111.
[8] 王 标, 李克智, 李贺军, 等(WANG Biao, et al). 无机材料学报(Journal of Inorganic Materials), 2007, 22 (4): 737-741.
[9] Huang J F, Zeng X R, Li H J, et al. Carbon, 2004, 42 (89): 1517-1521.
[10] Zhang Y L, Li H J, Fu Q G, et al. Surf. Coat. Technol., 2006, 201 (6): 3491-3495.
[11] Zhang Y L, Li H J, Fu Q G, et al. Carbon, 2007, 45 (5): 1130-1133.
[12] 孙万昌, 李贺军, 白瑞成, 等(SUN Wan-Chang, et al). 无机材料学报(Journal of Inorganic Materials), 2005, 20 (3): 671-676.
[13] 曾燮榕, 李贺军, 侯晏红, 等. 复合材料学报, 2000, 17 (2): 46-49.
[14] 孙万昌, 李贺军, 张秀莲. 航空学报, 2002, 20 (3): 276-278.
[15] 冼杏娟, 李端义. 复合材料破坏分析及微观图谱. 北京: 科学出版社, 1996. 57-58.
Outlines

/