Novel magneto-optical crystal YFeO3 (yttrium orthoferrite) was grown by the floating zone method. The growth parameters were optimized and YFeO3 single crystal up to 7--10mm in diameter and 60mm in length was obtained. XRD patterns show that it has orthorhombic perovskite structure with a=5.5964A, b=7.6052A, c=5.2842A. The solid-liquid interface is convex to the melt and the growth direction is close to [100] direction. No visible inclusions and grain boundaries are observed on the polished surface.

Cite this article

SHEN Hui , XU Jia-Yue , YU Jin-Xing , WU An-Hua . Floating Zone Growth of YFeO3 Single Crystals[J]. Journal of Inorganic Materials, 2007 , 22(6) : 1099 -1102 . DOI: 10.3724/SP.J.1077.2007.01099

References

[1] 刘湘林, 刘公强, 金绥更. 磁光材料和磁光器件, 第一版. 北京: 北京科学技术出版社, 1990. 30--32.
[2] 张溪文, 梁 军, 张守业(ZHANG Xi-Wen, et al). 无机材料学报(Journal of Inorganic Materials), 2003, 18 (4): 731--736.
[3] Didosyan Y S, Hauser H, Nicolics J, et al. J. Appl. Phys., 2000, 87 (9): 7079--7081.
[4] Didosyan Y S, Hauser H, Fiala W, et al. J. Appl. Phys., 2002, 91 (10): 7000--7002.
[5] Didosyan Y S, Hauser H. IEEE Trans. Instru. Meas., 2000, 49 (1): 14--18.
[6] Van Hook H J. J. Am. Ceram. Soc., 1962, 45: 162--165.
[7] Quon H H, Potvin A J. J. Crystal Growth, 1971, 10: 124--126.
[8] Wanklyn Barbara M. J. Crystal Growth, 1969, 5: 323--328.
[9] Kolb E D, Wood D L, Laudise R A. J. Appl. Phys., 1968, 39 (2): 1362--1364.
[10] Higuchi S, Yasunori F, Shunji T, et al. Jpn. J. Appl. Phys., 1999, 38: 4122--4126.
[11] Kitamura K, Kimura S. J. Crystal Growth, 1980, 48: 469--472.
Outlines

/