MoO3-V2O5-P2O5-Fe2O3玻璃的制备及性能研究

赵宏生1,2; 李艳青2; 周万城2; 罗发2; 唐春和1   

  1. 1. 清华大学核能与新能源技术研究院新材料研究室, 北京 102201; 2. 西北工业大学凝固技术国家重点实验室, 西安 710072
  • 收稿日期:2004-04-19 修回日期:2004-05-28 出版日期:2005-05-20 网络出版日期:2005-05-20

Preparation and Properties of MoO3-V2O5-P2O5-Fe2O3 Glasses

ZHAO Hong-Sheng1,2; LI Yan-Qing2; ZHOU Wan-Cheng2; LUO Fa2; TANG Chun-He1   

  1. 1.Division of New Materials; Institute of Nuclear and New Energy Technology; Tsinghua University; Beijing 102201; China; 2. State Key Laboratory of Solidification Processing; Northwestern Polytechnical University; Xi an 710072; China
  • Received:2004-04-19 Revised:2004-05-28 Published:2005-05-20 Online:2005-05-20

摘要: 制备了MoO3-V2O5-P2O5-Fe2O3系磷酸盐玻璃,研究了玻璃形成能力、热膨胀系数和抗潮解等性能.结果表明,MoO3-V2O5-P2O5-Fe2O3系统具有较宽的玻璃形成区和较强的玻璃形成能力,当MoO3/V2O5≈1.5时,玻璃形成能力最强. MoO3-V2O5-P2O5-Fe2O3玻璃的热膨胀系数约为60-110×10-7/℃,并且随着Fe2O3含量的增加而逐渐增大.加入适量的Fe2O3能够显著改善MoO3-V2O5-P2O5玻璃的抗潮解性能,在90℃的去离子水中的溶解速率达到8.0×10-9g·cm-2·min-1.

关键词: 磷酸盐玻璃, 玻璃形成能力, 热膨胀系数, 抗潮解

Abstract: Glasses in the MoO3-V2O5-P2O5-Fe2O3 quaternary system were prepared as potential replacements to lead-based frits for low
temperature sealing applications. The glass forming regions were explored and the glass forming ability, thermal expansion,
and water durability were investigated. Results show that MoO3-V2O5-P2O5 ternary system has strong glass forming ability, which extended down to
10mol% P2O5. The glass forming region in the MoO3-V2O5-P2O5-Fe2O3 quaternary system becomes relatively wider while the stabilities of the
glasses against crystallization are still strong with 10mol% Fe2O3. With the increasing content of Fe2O3 the glass forming region
becomes smaller. The glass forming ability in this quaternary system is most strong as the ratio of MoO3/V2O5 equals to 1.5.
The thermal expansion coefficient can be increased and the water durability improved by adding Fe2O3 content into the MoO3-V2O5-P2O5
ternary system. Trivalence iron ions can enter into phosphate chain and form Fe-O-P bond in place of P=O double bond, hereby increase the water durability
of glasses. Many glass compositions in the system of MoO3-V2O5-P2O5-Fe2O3 have a thermal expansion coefficient of 60~110×10-7/℃
and a dissolution rate in deionized water at 90℃ of 8.0×10-9g·cm-2·min-1, which willbe a good alternative to lead-based sealing frits.

Key words: phosphate glass, glass forming ability, thermal expansion, water durability