[1]Barsoum M W. Progress in Solid State Chemistry, 2000, 28(1-4):201-281. [2]朱教群,梅炳初,陈艳林.中国有色金属学报,2001,11(S2):29-32. [3]EL-Raghy S M, Waheed A F, EL-Raghy T S, et al.Journal of Materials Science Letters,1999,18(7):519-520. [4]Jovic V D, Jovic B M, Gupta S, et al. Corrosion Science,2006,48(12):4274-4282. [5]Travaglini J, Barsoum M W, Jovic V, et al. Corrosion Science,2003,45(6):1313-1327. [6]Hong XionLin, Mei BingChu, Zhu JiaoQun, et al.Journal of Materials Science,2004,39(5):1589-1592. [7]Zhou W B, Mei B C, Zhu J Q, et al. Materials Letters,2005,59(1):131-134. [8]周卫兵,梅炳初,朱教群,等.武汉理工大学学报,2002,24(9):22-24. [9]郭俊明,王宝森,陈克新,等.稀有金属材料与工程,2007,36(5):865-868. [10]Barsoum M W, ElRaghy T, Ogbuji L. Journal of the Electrochemical Society,1997,144(7):2508-2516. [11]梅炳初,徐学文,朱教群,等.稀有金属材料与工程,2005,34(6):895-898. [12]Schuter R, Thomas D S. Metals Handbook:Corrsion, ninth ed. ASM International,1987:680-704. [13]王 苹,梅炳初,洪小林,等.武汉理工大学学报,2007,29(4):5-7. [14]Lin Z J, Zhou M J, Zhou Y C, et al. Acta Material,2006,54(10):1009-1015. |