富铝CMAS对稀土硅酸盐环境障涂层的腐蚀行为与机制研究
范栋, 钟鑫, 王亚文, 张振忠, 牛亚然, 李其连, 张乐, 郑学斌

Corrosion Behavior and Mechanism of Aluminum-rich CMAS on Rare-earth Silicate Environmental Barrier Coatings:
FAN Dong, ZHONG Xin, WANG Yawen, ZHANG Zhenzhong, NIU Yaran, LI Qilian, ZHANG Le, ZHENG Xuebin
表5 图5中标记区域的EDS元素组成
Table 5 EDS elemental compositions of the marked regions in Fig. 5
EDS/
(%, in atom)
Gd Y Er Si O Ca Al Mg
Point 1 24.48 16.22 51.61 7.68
Point 2 1.05 12.62 59.63 14.25 9.78 2.66
Point 3 26.70 15.78 50.12 7.40
Point 4 17.10 8.23 51.25 2.92 16.41 4.09
Point 5 0.94 14.23 57.36 13.94 11.98 1.54
Point 6 28.80 12.77 52.22 6.22
Point 7 7.12 13.05 49.26 7.08 18.26 5.24