富铝CMAS对稀土硅酸盐环境障涂层的腐蚀行为与机制研究
|
|
范栋, 钟鑫, 王亚文, 张振忠, 牛亚然, 李其连, 张乐, 郑学斌
|
Corrosion Behavior and Mechanism of Aluminum-rich CMAS on Rare-earth Silicate Environmental Barrier Coatings:
|
|
FAN Dong, ZHONG Xin, WANG Yawen, ZHANG Zhenzhong, NIU Yaran, LI Qilian, ZHANG Le, ZHENG Xuebin
|
|
表4 中标记区域的EDS元素组成
|
Table 4 EDS elemental compositions of the marked regions in Fig. 4
|
|
| EDS/(%, in atom) | Gd | Y | Er | Si | O | Ca | Al | Mg | | Point 1 | 19.21 | — | —- | 11.70 | 60.65 | 8.44 | — | — | | Point 2 | 1.16 | — | — | 13.06 | 59.37 | 13.78 | 10.18 | 2.45 | | Point 3 | — | 15.29 | — | 16.00 | 61.82 | 6.89 | — | — | | Point 4 | — | 7.18 | — | 15.50 | 50.17 | 9.58 | 12.14 | 5.43 | | Point 5 | — | 0.96 | — | 13.56 | 59.62 | 13.03 | 10.40 | 2.42 | | Point 6 | — | — | 20.27 | 12.11 | 61.12 | 6.50 | — | — | | Point 7 | — | — | 8.70 | 10.95 | 59.15 | 8.09 | 10.95 | 4.65 | | Point 8 | — | — | 0.92 | 3.29 | 58.74 | 19.61 | 3.29 | 2.07 |
|
|
|