富铝CMAS对稀土硅酸盐环境障涂层的腐蚀行为与机制研究
范栋, 钟鑫, 王亚文, 张振忠, 牛亚然, 李其连, 张乐, 郑学斌

Corrosion Behavior and Mechanism of Aluminum-rich CMAS on Rare-earth Silicate Environmental Barrier Coatings:
FAN Dong, ZHONG Xin, WANG Yawen, ZHANG Zhenzhong, NIU Yaran, LI Qilian, ZHANG Le, ZHENG Xuebin
表3 图3中标记区域的EDS元素组成
Table 3 EDS elemental compositions of the marked regions in Fig. 3
EDS/
(%, in atom)
Gd Y Er Si O Ca Al Mg
Point 1 20.60 19.62 51.73 8.02
Point 2 26.04 17.55 50.57 5.83
Point 3 26.95 15.16 50.78 7.10
Point 4 14.03 5.72 52.27 4.01 20.31 3.66