Cansas-II SiCf/SiC复合材料的高温拉伸蠕变行为
|
荆开开, 管皞阳, 朱思雨, 张超, 刘永胜, 王波, 王晶, 李玫, 张程煜
|
Tensile Creep Behavior of Cansas-II SiCf/SiC Composites at High Temperatures
|
JING Kaikai, GUAN Haoyang, ZHU Siyu, ZHANG Chao, LIU Yongsheng, WANG Bo, WANG Jing, LI Mei, ZHANG Chengyu
|
|
表3 2D-SiCf/SiC复合材料在空气中的高温拉伸蠕变性能
|
Table 3 Tensile creep properties of 2D-SiCf/SiC composites in air at high temperatures
|
|
Specimen | Tempera- ture/℃ | Stress/ MPa | Steady-state creep strain rate/s-1 | Creep rupture time/h | Creep strain/% | 2D-SiCf/SiC | 1200 | 100 | 1.86×10-10 | >560 | 0.20 | 1200 | 110 | 4.95×10-10 | >560 | 0.23 | 1200 | 120 | 2.16×10-9 | 42 | 0.18 | 1200 | 140 | 8.45×10-7 | 0.1 | 0.21 | 1300 | 90 | 5.62×10-10 | >500 | 0.28 | 1300 | 100 | 1.73×10-9 | 70 | 0.20 | 1300 | 120 | 1.86×10-8 | 6 | 0.28 | 1400 | 80 | 1.32×10-9 | 88 | 0.33 | 1400 | 100 | 1.46×10-8 | 1.6 | 0.57 | CVI-SiCf/SiC[13] | 1300 | 75 | 2.3×10-9 | 111.1 | — | 1300 | 90 | 6.2×10-8 | 33.4 | — | 1300 | 120 | 3.6×10-7 | 0.83 | — | 1300 | 150 | 3.0×10-6 | 0.14 | — | MI-SiCf/SiC[15] | 1204 | 125 | 3.0×10-11 | >1000 | 0.25 | 1204 | 140 | 2.3×10-10 | >1000 | 0.31 | 1204 | 150 | — | 82.1 | 0.29 |
|
|
|