基于羟基磷灰石材料的风化脆弱骨质文物加固保护研究
刘妍1,2,3(), 张宇帆1,2,3, 王茜蔓1,2,3, 李婷1,2,3, 马文婷1,2,3, 杨富巍1,2,3(), 陈靓1,2,3, 赵东月1,2,3, 严小琴1,2,3
Consolidation of Fragile Weathered Bone Relics Using Hydroxyapatite Material as Consolidant
LIU Yan1,2,3(), ZHANG Yufan1,2,3, WANG Ximan1,2,3, LI Ting1,2,3, MA Wenting1,2,3, YANG Fuwei1,2,3(), CHEN Liang1,2,3, ZHAO Dongyue1,2,3, YAN Xiaoqin1,2,3

图9. 加固处理后脆弱骨样品显微形貌

Fig. 9. Morphologies of fragile bone samples after consolidation treatments with mass ratios of calcium oxide to calcium hydrogen phosphate at 1 : 1 (a), 1 : 3 (b), 1 : 4 (c), 1 : 5 (d), 1 : 6 (e) and 1 : 7 (f), respectively