[an error occurred while processing this directive]
基于羟基磷灰石材料的风化脆弱骨质文物加固保护研究
刘妍1,2,3(), 张宇帆1,2,3, 王茜蔓1,2,3, 李婷1,2,3, 马文婷1,2,3, 杨富巍1,2,3(), 陈靓1,2,3, 赵东月1,2,3, 严小琴1,2,3
Consolidation of Fragile Weathered Bone Relics Using Hydroxyapatite Material as Consolidant
LIU Yan1,2,3(), ZHANG Yufan1,2,3, WANG Ximan1,2,3, LI Ting1,2,3, MA Wenting1,2,3, YANG Fuwei1,2,3(), CHEN Liang1,2,3, ZHAO Dongyue1,2,3, YAN Xiaoqin1,2,3

图7. 加固处理方式和加固剂配比对脆弱骨样品表面强度的影响

Fig. 7. Effects of consolidation method and consolidant ratio on surface strength of the bones
(a) Consolidation way; (b) Consolidant ratio