表1 闪烧和传统烧结的实验参数
Table 1 Experimental parameters of flash sintering and conventional sintering
Label E/(V·cm-1) J/(mA·mm-2) Tf/℃ t Te/℃
F1 50 150 300 60 s 990
F2 50 200 300 60 s 1060
F3 50 250 300 60 s 1100
F4 50 300 300 60 s 1130
C1 - - 990 2 h -
C2 - - 1060 2 h -
C3 - - 1100 2 h -
C4 - - 1130 2 h -