L-3-(4-吡啶基)-丙氨酸钝化钙钛矿太阳电池界面缺陷
刘雯雯1(), 胡志蕾1, 王立1, 曹梦莎1, 张晶1, 张婧1, 张帅1(), 袁宁一1, 丁建宁2()
Passiviation of L-3-(4-Pyridyl)-alanine on Interfacial Defects of Perovskite Solar Cell
LIU Wenwen1(), HU Zhilei1, WANG Li1, CAO Mengsha1, ZHANG Jing1, ZHANG Jing1, ZHANG Shuai1(), YUAN Ningyi1, DING Jianning2()

图3. (a)钙钛矿薄膜的ATR-FT-IR光谱((b)为(a)中黑色虚线矩形区域的放大图), (c)薄膜的紫外-可见吸收光谱图和(d)XRD图谱

Fig. 3. (a) ATR-FT-IR spectra, ((b) magnified ATR-FT-LR spectra of rectangular area in (a)), (c) UV-Vis absorption spectra and (d) XRD patterns of FTO/TiO2/perovskite films with and without PLA