[an error occurred while processing this directive]
L-3-(4-吡啶基)-丙氨酸钝化钙钛矿太阳电池界面缺陷
刘雯雯1(), 胡志蕾1, 王立1, 曹梦莎1, 张晶1, 张婧1, 张帅1(), 袁宁一1, 丁建宁2()
Passiviation of L-3-(4-Pyridyl)-alanine on Interfacial Defects of Perovskite Solar Cell
LIU Wenwen1(), HU Zhilei1, WANG Li1, CAO Mengsha1, ZHANG Jing1, ZHANG Jing1, ZHANG Shuai1(), YUAN Ningyi1, DING Jianning2()

图2. (a, c, e)参照及(b, d, f)PLA修饰FTO/TiO2/钙钛矿薄膜的(a,b)表面、(c,d)截面SEM照片和(e,f)晶粒尺寸分布图

Fig. 2. (a,b) Surface and (c,d) cross sectional SEM images, (e,f) grain size distributions of FTO/TiO2/perovskite films (a, c, e) without and (b, d, f) with PLA