扩散应力诱导的锂离子电池失效机理研究进展
|
王亚楠 1,2,3(  ),李华 1,2,3,王正坤 1,厉青峰 1,练晨 1,何鑫 1
|
Progress on Failure Mechanism of Lithium Ion Battery Caused by Diffusion Induced Stress
|
WANG Yanan 1,2,3(  ),LI Hua 1,2,3,WANG Zhengkun 1,LI Qingfeng 1,LIAN Chen 1,HE Xin 1
|
|
图7. (a)双相脱嵌机制的球形颗粒的脱锂过程[35]; (b)双相脱嵌机制的球形颗粒锂化过程中的表面切向应力[36], 其中空心圆, 实心圆, 星号和星形分别代表颗粒的初始无量纲尺寸为0.01, 0.1, 1.0和10.0; (c)临界尺寸L与放电倍率的关系[42]
|
Fig. 7. (a) Delithiation process of spherical particle with two-phase deintercalation mechanism[35]; (b) Surface tangential stress of spherical particle during lithiation process with two-phase deintercalation mechanism[36], the hollow circle, solid circle, asterisk and star represent the initial dimensionless sizes of the particles as 0.01, 0.1, 1.0 and 10.0, respectively; (c) Relationship between critical dimension and discharge rate[42]
|
|
 |
|
|