Preparation of 0.84(K0.48Na0.52)NbO3-0.16K0.56Li0.38NbO2.97Lead-free Piezoelectric Ceramics by Multi-layer Process
ZHANG Zhi-Qiang1,2, LIU Zhi-Fu1, LI Yong-Xiang1
图2 不同烧结温度(1000 ℃和1050 ℃)和保温时间(8、15和30 min)下陶瓷样品的相对密度 Fig. 2 Relative density of KNN-KLN ceramics with different sintering temperatures 1000 ℃ and 1050 ℃ and holding times 8, 15 and 30 min